Which defect occurs as surface bubbles in FRP due to moisture in the laminate?

Study for the NHI Bridge Inspection Course 130055. Prepare with flashcards and multiple choice questions, each question includes hints and explanations. Ensure you're ready for your exam!

Multiple Choice

Which defect occurs as surface bubbles in FRP due to moisture in the laminate?

Explanation:
Moisture in FRP laminates can diffuse in and, if it becomes trapped under the surface resin, vaporize and pressurize between the layers. That gas buildup pushes the surface outward, creating bubbles or blisters on the exterior. This kind of defect is blistering because it’s literally a bubble on the surface caused by trapped moisture vapor. Other issues involve different failure modes—delamination is a separation between layers, cracking is cracks in the material, and pitting are small surface pits—not the gas-filled surface bubbles produced by moisture.

Moisture in FRP laminates can diffuse in and, if it becomes trapped under the surface resin, vaporize and pressurize between the layers. That gas buildup pushes the surface outward, creating bubbles or blisters on the exterior. This kind of defect is blistering because it’s literally a bubble on the surface caused by trapped moisture vapor. Other issues involve different failure modes—delamination is a separation between layers, cracking is cracks in the material, and pitting are small surface pits—not the gas-filled surface bubbles produced by moisture.

Subscribe

Get the latest from Examzify

You can unsubscribe at any time. Read our privacy policy